Excellent synergies of mechanical properties and biological performance of additively-manufactured Ti-Cu - Cu alloy

被引:0
|
作者
Gong, Tao [1 ]
Zhao, Qinyang [1 ]
Mao, Yamei [1 ]
Zhang, Yong [1 ]
Chen, Yongnan [1 ]
Zhang, Fengying [1 ]
Ma, Jingyu [1 ]
Wang, Lin [2 ]
Gao, Guangrui [3 ]
机构
[1] Changan Univ, Sch Mat Sci & Engn, Xian 710064, Peoples R China
[2] Beijing Inst Technol, Natl Key Lab Sci & Technol Mat Shock & Impact, Beijing 100081, Peoples R China
[3] Xian Surface Mat Protect Co Ltd, Xian 710018, Peoples R China
基金
中国国家自然科学基金;
关键词
Additive manufacturing; Microstructure evolution; Mechanical properties; Biological performance; Ti-cu alloy; BEARING TITANIUM-ALLOY; ANTIBACTERIAL PROPERTIES; HEAT-TREATMENT; COPPER; TI-6AL-4V; BEHAVIOR; SILVER; LASER; TEMPERATURE; EVOLUTION;
D O I
10.1016/j.matchar.2024.114255
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Insufficient combination of mechanical properties and biological performance has hindered the application expansion of Ti-Cu - Cu alloy in biomedical field. In this study, Ti-13Cu-1Al alloy was prepared by additive manufacturing technology, and the microstructure and properties of the alloy were regulated by post-heat treatment. The strengthening-toughening mechanisms and biological performance enhancing mechanisms were comprehensively revealed by investigating the microstructure and properties of the alloy. The results show that, although the as-deposited alloy has a homogeneous microstructure and fine precipitated phases, the higher residual stresses in the alloy make it poorly ductile. After annealing in the biphasic region, due to the processes of precipitated phases spheroidization, elimination of small defects and residual stresses, reduction of hard phases' volume fraction, and orientation alteration of the alpha-Ti matrix, the elongation of the alloy increases significantly up to 18%. After annealing in the beta-phase region, the morphology of Ti2Cu 2 Cu phases changed from blocky to lath, which effectively hinder dislocation motion and leads to a significant increase in the tensile strength, up to a maximum of 1025 MPa. Meanwhile, the alloy also has good plasticity due to the rich slip pattern of dislocations in alpha-Ti matrix, achieving a good balance of strength and plasticity. In addition, both the as-deposited and annealed alloy show strong bacterial inhibition and good biocompatibility comparing to as-cast alloy, indicating excellent synergies of mechanical and biological properties are achieved for the additively-manufactured alloy.
引用
收藏
页数:15
相关论文
共 50 条
  • [1] Antibacterial Ti-Cu alloy with enhanced mechanical properties as implant applications
    Yi, ChangBo
    Ke, ZunYun
    Zhang, Lei
    Tan, Jun
    Jiang, YeHua
    He, ZhengYuan
    MATERIALS RESEARCH EXPRESS, 2020, 7 (10)
  • [2] Controlling Intermetallic Compound Distribution in Additively Manufactured Ti-Cu Alloys by Heat Treatment
    Hanada H.
    Kariya S.
    Shitara K.
    Umeda J.
    Kondoh K.
    Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 2023, 70 (06): : 290 - 297
  • [3] Synergic enhancement of strength and ductility in wire arc additively manufactured Ti-Cu alloys
    Zheng, Zhendan
    Chen, Jiaming
    Yu, Peng
    Wu, Shaojie
    Cheng, Fangjie
    MATERIALS LETTERS, 2024, 377
  • [4] Achieve an excellent strength-ductility balance by introducing heterogeneous structure in wire arc additively manufactured Ti-Cu alloys
    Zheng, Zhendan
    Chen, Jiaming
    Yu, Peng
    Tian, Pengfei
    Wang, Haijie
    Wu, Shaojie
    Cheng, Fangjie
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2025, 927
  • [5] HEAT TREATMENT AND MECHANICAL PROPERTIES OF TI-CU ALLOYS
    HOLDEN, FC
    WATTS, AA
    OGDEN, HR
    JAFFEE, RI
    TRANSACTIONS OF THE AMERICAN INSTITUTE OF MINING AND METALLURGICAL ENGINEERS, 1955, 203 (01): : 117 - 125
  • [6] Mechanical properties and microstructures of cast Ti-Cu alloys
    Kikuchi, M
    Takada, Y
    Kiyosue, S
    Yoda, M
    Woldu, M
    Cai, Z
    Okuno, O
    Okabe, T
    DENTAL MATERIALS, 2003, 19 (03) : 174 - 181
  • [7] Microstructure and Mechanical Properties of Sintered Ti-Cu Alloys
    Pripanapong, P.
    Luangvaranunt, T.
    FUNCTIONALIZED AND SENSING MATERIALS, 2010, 93-94 : 99 - 104
  • [8] Biological corrosion behaviour and antibacterial properties of Ti-Cu alloy with different Ti2Cu morphologies for dental applications
    Xin, Cheng
    Wang, Nan
    Chen, Yongnan
    He, Binbin
    Zhao, Qinyang
    Chen, Lei
    Tang, Yufei
    Luo, Binli
    Zhao, Yongqing
    Yang, Xiaokang
    MATERIALS & DESIGN, 2022, 215
  • [9] PRECIPITATION HARDENING IN A TI-CU ALLOY
    HOWE, LM
    SAAREMA, E
    PARR, JG
    TRANSACTIONS OF THE AMERICAN INSTITUTE OF MINING AND METALLURGICAL ENGINEERS, 1956, 206 (05): : 512 - 513
  • [10] Synthesis of Ti-Cu Multiphase Alloy by Spark Plasma Sintering: Mechanical and Corrosion Properties
    Shichalin, Oleg O.
    Sakhnevich, Vladimir N.
    Buravlev, Igor Yu
    Lembikov, Aleksey O.
    Buravleva, Anastasia A.
    Azon, Semen A.
    Yarusova, Sofia B.
    Danilova, Sakhayana N.
    Fedorets, Alexander N.
    Belov, Anton A.
    Papynov, Evgeniy K.
    METALS, 2022, 12 (07)