Role of Quenching Temperature Selection in the Improvement of the Abrasive (Al2O3) Wear Resistance of Hybrid Multi-Component Cast Irons

被引:1
|
作者
Chabak, Yuliia [1 ,2 ]
Efremenko, Vasily [1 ,2 ]
Petryshynets, Ivan [2 ]
Golinskyi, Michail [1 ]
Shimizu, Kazumichi [3 ]
Efremenko, Bohdan [1 ,4 ]
Kudin, Vadim [5 ]
Azarkhov, Alexander [4 ]
机构
[1] Pryazovskyi State Tech Univ, Phys Dept, UA-49044 Dnipro, Ukraine
[2] Slovak Acad Sci, Inst Mat Res, Div Met Syst, Kosice 04001, Slovakia
[3] Muroran Inst Technol, Grad Sch Engn, 27-1 Mizumoto, Muroran, Hokkaido 0508585, Japan
[4] Pryazovskyi State Tech Univ, Biomed Engn Dept, UA-49044 Dnipro, Ukraine
[5] Natl Univ Zaporizhzhia Polytech, Dept Machines & Technol Foundry Prod, UA-69063 Zaporizhzhia, Ukraine
关键词
multi-component cast iron; high boron content; quenching; carboborides; matrix; hardness; abrasive wear resistance; HEAT-TREATMENT; MECHANICAL-PROPERTIES; CURIE-TEMPERATURE; HARDNESS; CARBIDES; BEHAVIOR; CR; MN; NI; MICROSTRUCTURE;
D O I
10.3390/ma17153742
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this paper, enhancing the tribological characteristics of novel cast metallic materials-hybrid multi-component cast irons-by applying a strengthening heat treatment is described. The experimental materials were the cast alloys of a nominal composition (5 wt.% W, 5 wt.% Mo, 5 wt.% V, 10 wt.% Cr, 2.5 wt.% Ti, Fe is a balance) supplemented with 0.3-1.1 wt.% C and 1.5-2.5 wt.% B (total of nine alloys). The heat treatment was oil-quenching followed by 200 degrees C tempering. The quench temperature (QT) varied in the range of 900-1200 degrees C, with a step of 50 degrees C (with a 2-h holding at QT). The correlation of the QT with microstructure and properties was estimated using microstructure/worn surface characterization, differential scanning calorimetry, hardness measurement, and three-body-abrasive wear testing (using Al2O3 particles). The as-cast alloys had a multi-phase structure consisting of primary and/or eutectic borocarbide M-2(B,C)(5), carboborides M(C,B), M-7(C,B)(3), M-3(C,B), and the matrix (ferrite, martensite, pearlite/bainite) in different combinations and volume fractions. Generally, the increase in the quenching temperature resulted in a gradual increase in hardness (maximally to 66-67 HRC) and a decrease in the wear rate in most alloys. This was due to the change in the phase-structure state of the alloys under quenching, namely, the secondary carboboride precipitation, and replacing ferrite and pearlite/bainite with martensite. The wear rate was found to be inversely proportional to bulk hardness. The maximum wear resistance was attributed to QT = 1150-1200 degrees C, when the wear rate of the alloys was lowered by three to six times as compared to the as-cast state. With the QT increase, the difference in the wear rate of the alloys decreased by three times. The highest abrasive resistance was attributed to the alloys with 1.1 wt.% C, which had a 2.36-3.20 times lower wear rate as compared with that of the reference alloy (13 wt.% Cr cast iron, hardness of 66 HRC). The effects of carbon and boron on hardness and wear behavior are analyzed using the regression models developed according to the factorial design procedure. The wear mechanisms are discussed based on worn surface characterization.
引用
收藏
页数:26
相关论文
共 50 条
  • [1] Three body type abrasive wear characteristics of multi-component white cast irons
    Kusumoto, Kenta
    Shimizu, Kazumichi
    Efremenko, V. G.
    Hara, Hiroya
    Shirai, Masato
    Ito, Jun
    Hatate, Minoru
    Gaqi, Yila
    Purba, Riki Hendra
    WEAR, 2019, 426 : 122 - 127
  • [2] Erosive Wear Characteristics of High Cr Multi-Component White Cast Irons at Elevated Temperature
    Huq, Mohammad Jobayer
    Shimizu, Kazumichi
    Kusumoto, Kenta
    Purba, Riki Hendra
    Gaqi, Yila
    INTERNATIONAL JOURNAL OF METALCASTING, 2024,
  • [3] Improving wear and corrosion resistance of Ti-alloyed nodular cast irons by Al2O3 and SiC-reinforced Al2O3 coatings
    Kurtulus, Volkan
    Gorgulu, Burak
    Eraslan, Fatma Sezgi
    Gecu, Ridvan
    SURFACE & COATINGS TECHNOLOGY, 2025, 498
  • [4] Effects of C and W Contents and Heat Treatment Condition on Microstructure and Wear Resistance of Multi-Component White Cast Irons
    Pan, E. N.
    Chang, W. S.
    Sasaguri, N.
    Matsubara, Y.
    TRANSACTIONS OF THE AMERICAN FOUNDRY SOCIETY, VOL 117, 2009, 117 : 463 - +
  • [5] Abrasive wear properties of Al2O3/Mo composite
    Hou, Fengliang
    Ni, Feng
    Cui, Yansui
    Hou, Maizhen
    Wei, Shizhong
    Xu, Liujie
    Fuhe Cailiao Xuebao/Acta Materiae Compositae Sinica, 2011, 28 (04): : 136 - 141
  • [6] Effect of superficial residual stresses on abrasive wear resistance of Al2O3/Al2O3+3Y-TZP multilayers
    de Portu, G
    Micele, L
    Prandstraller, D
    Palombarini, G
    Pezzotti, G
    NEW FRONTIERS OF PROCESSING AND ENGINEERING IN ADVANCED MATERIALS, 2005, 502 : 217 - 222
  • [7] Evaluation of Abrasive Wear Resistance of Al2O3/7075 Composite by Taguchi Experimental Design Technique
    Sardar, Santanu
    Karmakar, Santanu Kumar
    Das, Debdulal
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2018, 71 (08) : 1847 - 1858
  • [8] The abrasive wear study of a Ni3Al/Al2O3 composite material
    Hu, CT
    Chiou, WC
    ROLL OF CHARACTERIZATION IN UNDERSTANDING ENVIRONMENTAL DEGRADATION OF MATERIALS, 1998, 25 : 177 - 182
  • [9] Evaluation of Abrasive Wear Resistance of Al2O3/7075 Composite by Taguchi Experimental Design Technique
    Santanu Sardar
    Santanu Kumar Karmakar
    Debdulal Das
    Transactions of the Indian Institute of Metals, 2018, 71 : 1847 - 1858
  • [10] Influence of Al2O3 reinforcement on the abrasive wear characteristic of Al2O3/PA1010 composite coatings
    Jia, X
    Ling, XM
    WEAR, 2005, 258 (09) : 1342 - 1347