Poly(ethylene 2,5-furandicarboxylate) pole figures to determine the microstructural scheme upon uniaxial stretching: Link between orientation and crystallisation

被引:0
|
作者
Forestier, Emilie [1 ,2 ,3 ]
Combeaud, Christelle [1 ]
Guigo, Nathanael [2 ]
Sbirrazzuoli, Nicolas [2 ]
Monge, Gabriel [1 ]
Haudin, Jean-Marc [1 ]
机构
[1] PSL Univ, Ctr Mat Forming CEMEF, Mines Paris, UMR CNRS 7635, F-06904 Sophia Antipolis, France
[2] Univ Cote Azur, Inst Chim Nice ICN, CNRS, UMR 7272, F-06108 Nice 2, France
[3] Agence Environm & Maitrise Energie, 20 Ave Gresille,BP 90406, F-49004 Angers 01, France
关键词
Poly(ethylene 2; 5-furandicarboxylate); Pole figures; Crystalline orientation; Microstructural development; Strain-induced crystallisation (SIC); NONISOTHERMAL CRYSTALLIZATION; THERMAL-BEHAVIOR; WATER SORPTION; FURANOATE); TRANSPORT; POLY(ETHYLENE-2,5-FURANOATE); POLY(ETHYLENE-TEREPHTHALATE); CRYSTALLINITY; DYNAMICS; MOBILITY;
D O I
10.1016/j.polymer.2024.127613
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The emergent biobased polymer poly (ethylene 2,5-furandicarboxylate), PEF, has been studied through an innovative approach based on pole figures and orientation factor calculation. PEF uniaxial stretching was performed with different mechanical conditions (different equivalent strain rates), up to several levels of strain and while considering different post-stretching cooling conditions (interrupted, unloaded and ruptured samples). Samples were stretched and interrupted before and after the Natural Draw Ratio (NDR), the deformation for which the material starts strain-hardening. When PEF strain-hardens, it reveals both an increase of the crystalline orientation and crystallinity ratio with the deformation imposed. Unloading the material at temperature tends to decrease partially crystalline orientation, especially regarding the aliphatic part of the chains. Moreover, stretching PEF up to high strains, superior to the NDR, leads to crystal fragmentation. After all, all experimental results were compared to a texture model. It appears that a texture can be developed upon stretching that is close to a fibre texture, as the furan cycles tend to be parallel to the specimen plane.
引用
收藏
页数:10
相关论文
共 4 条
  • [1] Conformational Change Analysis of Poly(ethylene 2,5-furandicarboxylate) and Poly(ethylene terephthalate) under Uniaxial Stretching
    Forestier, Emilie
    Guigo, Nathanael
    Combeaud, Christelle
    Billon, Noelle
    Sbirrazzuoli, Nicolas
    MACROMOLECULES, 2020, 53 (19) : 8693 - 8703
  • [2] Biaxial Orientation of Poly(ethylene 2,5-furandicarboxylate): An Explorative Study
    van Berkel, Jesper G.
    Guigo, Nathanael
    Kolstad, Jeffrey J.
    Sbirrazzuoli, Nicolas
    MACROMOLECULAR MATERIALS AND ENGINEERING, 2018, 303 (03)
  • [3] A proposal for enhanced microstructural development of Poly(ethylene 2,5-furandicarboxylate), PEF, upon stretching: On strain-induced crystallization and amorphous phase stability improvement
    Forestier, Emilie
    Combeaud, Christelle
    Guigo, Nathanael
    Sbirrazzuoli, Nicolas
    POLYMER, 2022, 246
  • [4] Relationships between crystalline structure and the thermal behavior of poly(ethylene 2,5-furandicarboxylate): An in situ simultaneous SAXS-WAXS study
    Stoclet, Gregory
    Arias, Andrea
    Yeniad, Bahar
    De Vos, Sicco
    POLYMER ENGINEERING AND SCIENCE, 2019, 59 (08): : 1667 - 1677