Mechanochemical Synthesis of Cross-Linked Chitosan and Its Application as Adsorbent for Removal of Per- and Polyfluoroalkyl Substances from Simulated Electroplating Wastewater
被引:1
|作者:
Cagnetta, Giovanni
[1
,2
]
Yin, Zhou
[2
]
Qiu, Wen
[2
]
Vakili, Mohammadtaghi
[3
]
机构:
[1] Southwest Jiaotong Univ, Fac Geosci & Environm Engn, Chengdu 610031, Peoples R China
[2] Tsinghua Univ, Sch Environm, State Key Joint Lab Environm Simulat & Pollut Cont, Beijing Key Lab Emerging Organ Contaminants Contro, Beijing 100084, Peoples R China
[3] ORLEN UniCRE as, Revolucni 1521-84, Usti Nad Labem 40001, Czech Republic
来源:
关键词:
chitosan;
mechanochemical synthesis;
cross-linking;
adsorption;
PFAS;
DESTRUCTION;
NANO;
D O I:
10.3390/ma17123006
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
Chitosan is a promising adsorbent for removing a wide range of pollutants from wastewater. However, its practical application is hindered by instability in acidic environments, which significantly impairs its adsorption capacity and limits its utilization in water purification. While cross-linking can enhance the acid stability of chitosan, current solvent-based methods are often costly and environmentally unfriendly. In this study, a solvent-free mechanochemical process was developed using high-energy ball milling to cross-link chitosan with various polyanionic linkers, including dextran sulfate (DS), poly[4-styrenesulfonic acid-co-maleic acid] (PSSM), and tripolyphosphate (TPP). The mechanochemically cross-linked (MCCL) chitosan products exhibited superior adsorption capacity and stability in acidic solutions compared to pristine chitosan. Chitosan cross-linked with DS (Cht-DS) showed the highest Reactive Red 2 (RR2) adsorption capacity, reaching 1559 mg center dot g(-1) at pH 3, followed by Cht-PSSM (1352 mg center dot g(-1)) and Cht-TPP (1074 mg center dot g(-1)). The stability of MCCL chitosan was visually confirmed by the negligible mass loss of Cht-DS and Cht-PSSM tablets in pH 3 solution, unlike the complete dissolution of the pristine chitosan tablet. The MCCL significantly increased the microhardness of chitosan, with the order Cht-DS > Cht-PSSM > Cht-TPP, consistent with the RR2 adsorption capacity. When tested on simulated rinsing wastewater from chromium electroplating, Cht-DS effectively removed Cr(VI) (98.75% removal) and three per- and polyfluoroalkyl substances (87.40-95.87% removal), following pseudo-second-order adsorption kinetics. This study demonstrates the potential of the cost-effective and scalable MCCL approach to produce chitosan-based adsorbents with enhanced stability, mechanical strength, and adsorption performance for treating highly acidic industrial wastewater containing a mixture of toxic pollutants.