Influence of annealing temperature on microstructural evolution and tensile behavior of Ti-6Al-4V alloy manufactured by multi-directional forging

被引:1
|
作者
Liu, Shi-Shuang [1 ]
Cai, Jian-Ming [1 ]
Zhou, Yi [1 ]
Cao, Jing-Xia [1 ]
Zhang, Wang-Feng [1 ]
Dai, Sheng-Long [1 ]
Huang, Xu [1 ]
Cao, Chun-Xiao [1 ]
机构
[1] AECC Beijing Inst Aeronaut Mat, Aviat Key Lab Sci & Technol Adv Titanium Alloys, Beijing 100095, Peoples R China
关键词
Ti-6Al-4V forging; annealing temperature; microstructural evolution; secondary alpha phase; tensile properties; ductile fracture; AGING HEAT-TREATMENT; MECHANICAL-PROPERTIES; TEXTURE; TORSION; POWDER; STRAIN;
D O I
10.1016/S1003-6326(24)66512-X
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
A range of annealing treatments were implemented to regulate the microstructure and mechanical properties of Ti-6Al-4V forging. The results show that both the as-forged and as-annealed microstructures exhibit a bimodal structure composed of equiaxed primary alpha phase (alpha p) and transformed /3 phase (/3t). With the increase of annealing temperature, the secondary alpha (alpha s) phase precipitates from the /3 phase. There is no obvious texture and the crystal orientation is uniformly distributed. Meanwhile, strength initially increases and then decreases, whereas ductility remains largely unaffected. The alloy annealed at 860 degrees C has an excellent combination of strength and ductility, due to the larger content of the fine alpha s phase. All fracture surfaces contain massive dimples, which is a typical ductile fracture feature. The characteristics of microcracks, microvoids, and kinked alpha p/alpha l (equiaxed alpha p and lamellar alpha phase) phases are found near the fracture.
引用
收藏
页码:1864 / 1877
页数:14
相关论文
共 50 条
  • [1] Numerical Investigation on the Strain Evolution of Ti-6Al-4V Alloy during Multi-directional Forging at Elevated Temperatures
    Yan, Chenkan
    Shen, Jun
    Lin, Peng
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2018, 37 (06) : 571 - 580
  • [2] The role of microstructural evolution on the fatigue behavior of additively manufactured Ti-6Al-4V alloy
    Naab, Bryan
    Celikin, Mert
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 859
  • [4] New model of microstructural evolution during isothermal forging of Ti-6Al-4V alloy
    Li, MQ
    Xiong, AM
    MATERIALS SCIENCE AND TECHNOLOGY, 2002, 18 (02) : 212 - 214
  • [5] High Temperature Forming of Ti-6Al-4V Alloy Considering Microstructural Evolution
    Lee, YH
    Lee, CS
    Shin, TJ
    Hwang, SM
    Shim, IO
    ADVANCES IN ENGINEERING PLASTICITY AND ITS APPLICATIONS, PTS 1 AND 2, 2004, 274-276 : 117 - 122
  • [6] Microstructural evolution of a Ti-6Al-4V alloy produced by forging process combined with torsional motion
    Ohnishi, Hatsumi
    Takamoto, Kazuki
    Matsumoto, Hiroaki
    Matsumoto, Ryo
    JOURNAL OF MANUFACTURING PROCESSES, 2020, 58 : 1161 - 1170
  • [7] Superplastic deformation and microstructural evolution of Ti-6Al-4V alloy
    Zhu, Tangkui
    Li, Miaoquan
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2012, 41 (11): : 1970 - 1974
  • [8] Superplastic Deformation and Microstructural Evolution of Ti-6Al-4V Alloy
    Zhu Tangkui
    Li Miaoquan
    RARE METAL MATERIALS AND ENGINEERING, 2012, 41 (11) : 1970 - 1974
  • [9] Microstructural evolution,tensile property and dynamic compressive property of FSWed Ti-6Al-4V alloy
    Jia-Wei Bao
    Su-Yuan Yang
    Ting Yang
    Rare Metals, 2020, 39 (02) : 169 - 175
  • [10] Microstructural evolution, tensile property and dynamic compressive property of FSWed Ti-6Al-4V alloy
    Bao, Jia-Wei
    Yang, Su-Yuan
    Yang, Ting
    RARE METALS, 2020, 39 (02) : 169 - 175