Spray-Flame Synthesis of NASICON-Type Rhombohedral (α) Li1+xYxZr2-x(PO4)3 [x=0-0.2] Solid Electrolytes

被引:3
|
作者
Ali, Md Yusuf [1 ]
Chen, Tianyu [1 ]
Orthner, Hans [1 ]
Wiggers, Hartmut [1 ,2 ]
机构
[1] Univ Duisburg Essen, Inst Energy & Mat Proc React Fluids, D-47057 Duisburg, Germany
[2] Ctr Nanointegrat Duisburg Essen, CENIDE, D-47057 Duisburg, Germany
关键词
spray-flame synthesis; solid-state electrolyte; NASICON type Li1+xYxZr2-x(PO4)(3); nanoparticles; Li-ion batteries; ELECTRICAL-PROPERTIES; BATTERIES; ZIRCONIA; LIZR2(PO4)(3); TRANSFORMATION; NANOPARTICLES; CONDUCTIVITY; PYROLYSIS; KINETICS; MOBILITY;
D O I
10.3390/nano14151278
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Since solid electrolytes have a broad electrochemical stability window, are exceptionally electrochemically stable against Li metal, and function as a physical separator to prevent dendrite growth, they are at the forefront of alternate possibilities, further increasing the stability and energy density of Li-ion batteries. NASICON-type electrolytes are a promising candidate due to their negligible moisture sensitivity, which results in outstanding stability and a lower probability of Li2CO3 passivity under the ambient atmosphere. However, one of the most promising representatives, Li1+xYxZr2-x(PO4)(3) (LYZP), has multiple stable phases with significant variation in their corresponding Li-ion conductivity. In this paper, we have successfully synthesized the highly ionically conductive rhombohedral phase of LYZP via spray-flame synthesis. Two different solvent mixtures (e.g., 2-ethyl hexanoic acid/ethanol, propanol/propanoic acid) were chosen to explore the effect of precursor composition and combustion enthalpy on the phase composition of the nanoparticle. The as-synthesized nanoparticles from spray-flame synthesis consisted of the crystalline tetragonal zirconia (t-ZrO2) phase, while lithium, yttrium, and phosphate were present on the nanoparticles' surface as amorphous phases. However, a short annealing step (1 h) was sufficient to obtain the NASICON phase. Moreover, we have shown the gradual phase conversion from orthorhombic beta phase to rhombohedral alpha phase as the annealing temperature increased from 700 degrees C to 1300 degrees C (complete removal of beta phase). In this context, Y3+ doping was also crucial, along with the appropriate solvent mixture and annealing temperature, for obtaining the much-desired rhombohedral alpha phase. Further, 0.2 at% Y-3+ doping was added to the solvent mixture of 2-ethyl hexanoic acid/ethanol, and annealing at 1300 degrees C for 1 h resulted in a high ionic conductivity of 1.14 center dot 10(-5) S cm(-1).
引用
收藏
页数:19
相关论文
共 50 条
  • [1] Synthesis and Properties of NASICON-type Li1+xErxZr2-x(PO4)3 (0.1≤x≤0.2) Solid Electrolyte
    Liu Meijing
    Wei Hongkang
    Wang Chang'an
    RARE METAL MATERIALS AND ENGINEERING, 2015, 44 : 113 - 115
  • [2] Rhombohedral Li1+xYxZr2-x(PO4)3 Solid Electrolyte Prepared by Hot-Pressing for All-Solid-State Li-Metal Batteries
    Li, Qinghui
    Xu, Chang
    Huang, Bing
    Yin, Xin
    MATERIALS, 2020, 13 (07)
  • [3] High lithium-ion conducting NASICON-type Li1+x - yAlxNbyTi2-x - y(PO4)3 solid electrolytes
    Shang, Xuefu
    Nemori, Hiroyoshi
    Mitsuoka, Shigehi
    Mastuda, Yasuaki
    Takeda, Yasuo
    Yamamoto, Osamu
    Imanishi, Nobuyuki
    SOLID STATE IONICS, 2016, 297 : 43 - 48
  • [4] Li1+xAlxTi2-x (PO4)3, NASICON-type solid electrolyte fabrication with different methods
    Tolganbek, Nurbol
    Mentbayeva, Almagul
    Uzakbaiuly, Berik
    Kanamura, Kiyoshi
    Bakenov, Zhumabay
    MATERIALS TODAY-PROCEEDINGS, 2020, 25 : 97 - 100
  • [5] A microcontact impedance study on NASICON-type Li1+xAlxTi2-x(PO4)3 (0 ≤ x ≤ 0.5) single crystals
    Rettenwander, D.
    Welzl, A.
    Pristat, S.
    Tietz, F.
    Taibl, S.
    Redhammer, G. J.
    Fleig, J.
    JOURNAL OF MATERIALS CHEMISTRY A, 2016, 4 (04) : 1506 - 1513
  • [6] NASICON-Type Li1+xAlxZryTi2-x-y(PO4)3 Solid Electrolytes: Effect of Al, Zr Co-Doping and Synthesis Method
    Stenina, Irina
    Pyrkova, Anastasia
    Yaroslavtsev, Andrey
    BATTERIES-BASEL, 2023, 9 (01):
  • [7] High Li+ conduction in NASICON-type Li1+x,YxZr2-x(PO4)3 at room temperature
    Li, Yutao
    Liu, Meijing
    Liu, Kai
    Wang, Chang-An
    JOURNAL OF POWER SOURCES, 2013, 240 : 50 - 53
  • [8] Distribution and mobility of lithium in NASICON-type Li1-xTi2-xNbx(PO4)3 (0 ≤ x ≤ 0.5) compounds
    Kahlaoui, Radhouene
    Arbi, Kamel
    Jimenez, Ricardo
    Sobrados, Isabel
    Sanz, Jesus
    Ternane, Riadh
    MATERIALS RESEARCH BULLETIN, 2018, 101 : 146 - 154
  • [9] Study of the glass-to-crystal transformation of the NASICON-type solid electrolyte Li1+xAlxGe2 - x(PO4)3
    Liu, Zhongqing
    Venkatachalam, Sabarinathan
    Kirchhain, Holger
    van Wuellen, Leo
    SOLID STATE IONICS, 2016, 295 : 32 - 40
  • [10] Synthesis and ionic conductivity of (NH4)1–xHxHf2(PO4)3 (x = 0–1) NASICON-type materials
    M. A. Moshareva
    S. A. Novikova
    A. B. Yaroslavtsev
    Inorganic Materials, 2016, 52 : 1283 - 1290