Development of Low Anisotropic Commercially Pure Titanium Foils by Asymmetric Rolling and Annealing

被引:0
|
作者
Guo, Baohong [1 ,2 ]
Wang, Wenshuai [1 ,2 ]
Kong, Bin [3 ]
Wang, Zhengyu [4 ]
Kong, Charlie [5 ]
Yu, Hailiang [1 ,2 ]
机构
[1] Cent South Univ, Light Alloy Res Inst, Changsha 410083, Peoples R China
[2] Cent South Univ, State Key Lab Precis Mfg Extreme Serv Performance, Changsha 410083, Peoples R China
[3] Hunan Xiangtou Goldsky Titanium Met Co Ltd, Changsha 410205, Peoples R China
[4] Shimadzu China Co Ltd, Shanghai 200233, Peoples R China
[5] Univ New South Wales, Mark Wainwright Analyt Ctr, Sydney, NSW 2052, Australia
关键词
anisotropy; asymmetric rolling; microstructure; pure titanium; texture; MECHANICAL-PROPERTIES ANISOTROPY; PHASE-TRANSFORMATION; ALLOY; TEXTURE; TENSILE; DEFORMATION; FORMABILITY; EVOLUTION; BEHAVIOR; MICROSTRUCTURE;
D O I
10.1002/adem.202400248
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This work studies the evolution of microstructure, texture, and anisotropy of pure titanium foils by symmetric rolling (SR) and asymmetric rolling (ASR) and subsequent annealing. The as-received material shows equiaxed alpha grains and strong transverse texture (S-T texture), which leads to severe anisotropy. The index of plane anisotropy (IPA) of yield stress (YS) and ultimate tensile stress (UTS) of the as-received material is 15.2% and 7.5%, respectively. With the increase of deformation, the S-T texture is mainly transformed into a mixed texture of transverse texture (T texture) and rolling direction texture (R texture), which balances the start-up of the slip system when loading in the rolling direction (RD) and transverse direction (TD), so that the mechanical stress along RD and TD are close to each other and the anisotropy is improved. Especially for the samples prepared by ASR and annealing, the appearance of more R texture or basal texture (B texture) at the same deformation makes them show lower anisotropy. Therefore, after the same annealing treatment, the IPA of titanium foil with a thickness of 0.2 mm prepared by ASR is the smallest, which is 6.6% and 0.03%, respectively, while the IPA prepared by SR is 10.5% and 2.5%. The anisotropy of commercially pure titanium foil by symmetric rolling, asymmetric rolling (ASR) and subsequent annealing is studied. With the increase of deformation, the anisotropy decreased gradually. The reduction of anisotropy by ASR was more obvious. Meanwhile, ASR has a faster thinning ability, so it is an effective method for titanium foil processing.image (c) 2024 WILEY-VCH GmbH
引用
收藏
页数:13
相关论文
共 50 条
  • [1] Anisotropic tensile and ratcheting behavior of commercially pure titanium processed via cross rolling and annealing
    Ghosh, Atasi
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2019, 120 : 12 - 22
  • [2] Microstructure and textural evolution during cold rolling and annealing of commercially pure titanium sheet
    Liu, Na
    Wang, Ying
    He, Wei-jun
    Li, Jun
    Chapuis, Adrien
    Luan, Bai-feng
    Liu, Qing
    [J]. TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2018, 28 (06) : 1123 - 1131
  • [3] Effect of rolling mode and annealing temperature on microstructure and texture of commercially pure-titanium
    Ghosh, Atasi
    Singh, Amit
    Gurao, N. P.
    [J]. MATERIALS CHARACTERIZATION, 2017, 125 : 83 - 93
  • [4] Blue Diode Laser Welding of Commercially Pure Titanium Foils
    Pasang, Tim
    Lin, Pai-Chen
    Misiolek, Wojciech Z.
    Wei, Jia-Yuan
    Masuno, Shinichiro
    Tsukamoto, Masahiro
    Hori, Eiji
    Sato, Yuji
    Tao, Yuan
    Yudhistiro, Danang
    Yunus, Salahuddin
    [J]. QUANTUM BEAM SCIENCE, 2022, 6 (03)
  • [5] HOT-ROLLING TEXTURE OF COMMERCIALLY PURE TITANIUM
    SHINDO, T
    [J]. TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 71 : 1625 - 1625
  • [6] Effect of Asymmetric Cold Rolling on Texture of a Commercially Pure Copper
    Uniwersal, A.
    Wrobel, M.
    Wierzbanowski, K.
    Wronski, M.
    [J]. ACTA PHYSICA POLONICA A, 2016, 130 (04) : 1049 - 1052
  • [7] Effect of cold rolling on the transition texture of commercially pure titanium
    Gey, N
    Humbert, M
    Singh, AK
    [J]. JOURNAL DE PHYSIQUE IV, 2001, 11 (PR4): : 91 - 98
  • [8] COLD-ROLLING PROPERTIES OF COMMERCIALLY PURE TITANIUM STRIP
    FUKUDA, M
    [J]. TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (05): : S734 - S734
  • [9] Combined effects of low temperature nitriding and cold rolling on fatigue properties of commercially pure titanium
    Kikuchi, Shoichi
    Ueno, Akira
    Akebono, Hiroyuki
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2020, 139
  • [10] Constitutive Analysis of the Anisotropic Flow Behavior of Commercially Pure Titanium
    Kim, Daehwan
    Lee, Taekyung
    Lee, Chong Soo
    [J]. APPLIED SCIENCES-BASEL, 2020, 10 (22): : 1 - 7