Durability deterioration and corrosion mechanism of shotcrete in salt lake environment

被引:0
|
作者
Wang, Jiabin [1 ,3 ]
Niu, Ditao [2 ,3 ]
He, Hui [1 ]
Song, Zhanping [2 ]
机构
[1] Xi'an Technological University, Xi'an,710021, China
[2] College of Civil Engineering, Xi'an University of Architecture and Technology, Xi'an,710055, China
[3] Key Laboratory of Green Building in West China, Xi'an University of Architecture and Technology, Xi'an,710055, China
关键词
D O I
暂无
中图分类号
学科分类号
摘要
Salt lake is widely distributed in western China. The high concentrations of chlorine salt, sulfate, and magnesium salt in the soil and groundwater are the major causes leading to the deterioration of lining shotcrete and the corrosion of reinforcement. In order to systematically study the deterioration rules and mechanism of the durability of shotcrete lining in salt lake corrosion environment, the dry-wet alternate method was employed to simulate the corrosion of tunnel lining, and the durability experiment of shotcrete was carried out with 5%Na2SO4+5%MgSO4+3.5%NaCl mixed solution. Relative dynamic elastic modulus, mass change and relative compressive strength were measured. After experiencing corrosion, mineral composition and microstructure of corrosion products, pore structure and ion content were tested by using XRD, TG-DSC, SEM & EDX, liner traverse method and electrochemical method. Acid-soluble sulfate content may obviously increase with the increase of the dry-wet cycles, and water-soluble chloride and sodium content slowly increased. However, the pH value of water-soluble calcium and concrete may decrease. The corrosion process of shotcrete is composed of three stages, including the formation stage of brucite, gypsum and ettringite, the stage of C-S-H decomposition and thaumasite formation, and the formation stage of M-S-H. Eventually, under the coactions of swelling stress and crystallization pressure from thaumasite, brucite, gypsum, ettringite and crystallized salt, the amount of pores and air content in shotcrete were increased, so that the formation of netty cracks could result in the quick deterioration of shotcrete in physical and mechanical properties. The microcracks of mould concrete quickly propagated under the crystallization pressure of salt and truned to macrocracks after being connected with pores. Steel fibers can remarkably alleviate the internal stress of shotcrete, and hence can improve the corrosion resistance of shotcrete. © 2019, Editorial Office of China Civil Engineering Journal. All right reserved.
引用
收藏
页码:67 / 80
相关论文
共 50 条
  • [1] Durability performance of brine-exposed shotcrete in salt lake environment
    Wang, Jiabin
    Niu, Ditao
    Wang, Yan
    Wang, Bin
    CONSTRUCTION AND BUILDING MATERIALS, 2018, 188 : 520 - 536
  • [2] Analysis of corrosion mechanism and deterioration process for dowel under de-icing salt environment
    Li, L.-K. (llk217@126.com), 1600, Tsinghua University (30):
  • [3] Durability degradation of lining shotcrete exposed to compound salt
    Wang, Jiabin
    Niu, Ditao
    He, Hui
    Wang, Bin
    Tumu Gongcheng Xuebao/China Civil Engineering Journal, 2019, 52 (09): : 79 - 90
  • [4] Durability of steel fibre reinforced shotcrete with regard to corrosion
    Nordstrom, E
    SHOTCRETE: ENGINEERING DEVELOPMENTS, 2001, : 213 - 217
  • [5] Comprehensive assessment of the durability deterioration of asphalt pavement in salt environment: A literature review
    Jiang, Qi
    Chen, Meizhu
    Zhao, Yuechao
    Wu, Shaopeng
    Fan, Yansong
    Gan, Zhengxu
    Zhang, Yunlong
    CASE STUDIES IN CONSTRUCTION MATERIALS, 2022, 17
  • [6] Study on durability and damage mechanism of concrete exposed to salt lake conditions
    Yu, HF
    Sun, W
    Ma, HY
    ICACS 2003: INTERNATIONAL CONFERENCE ON ADVANCES IN CONCRETE AND STRUCTURES, VOL 1 AND 2, 2003, 32 : 391 - 398
  • [7] Concrete Durability in Urmia Lake: A case study of corrosion in a highly salty environment
    Ramezanianpour, Aliakbar
    Faridafshin, Farzad
    Mousavi, Mir Emad
    Concrete International, 2007, 29 (06) : 52 - 56
  • [8] Corrosion environment and concrete deterioration mechanism of shaft wall in coal mines
    Xie H.
    Lv H.
    Arabian Journal of Geosciences, 2021, 14 (11)
  • [9] Ion diffusion in shotcrete lining under compound salt corrosion environment saline soil in Northwest China
    Wang, Jiabin
    Zhang, Kaifeng
    Hou, Zeyu
    Niu, Ditao
    Tumu Gongcheng Xuebao/China Civil Engineering Journal, 2020, 53 (11): : 21 - 35
  • [10] Corrosion Investigation of Reinforced Concrete Under Qinghai Salt Lake Environment By EIS
    Liu, Qing
    Chen, Bokun
    Li, Ying
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2016, 11 (12): : 10238 - 10245