High-Strength Wear-Resistant Cu/Tungsten Carbide/Diamond Composites Fabricated by Powder Metallurgy

被引:1
|
作者
Zhang, Xiaoyan [1 ]
Lei, Qian [1 ]
Gao, Yang [1 ]
Zhou, Shijie [2 ]
Qiu, Wenting [3 ]
机构
[1] Cent South Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
[2] Zhengzhou Wode Superhard Mat Co Ltd, Zhenzhou 450041, Peoples R China
[3] Cent South Univ, Sch Mat Sci & Engn, Changsha 410083, Peoples R China
基金
中国国家自然科学基金;
关键词
Cu/tungsten carbide/diamond composites; molecular dynamics simulations; powder metallurgies; wear resistance; THERMAL-CONDUCTIVITY; TRIBOLOGICAL PROPERTIES; MECHANICAL-PROPERTIES; CU; MATRIX; BEHAVIOR; MICROSTRUCTURE; NANOCOMPOSITES; CONDUCTANCE; CARBIDES;
D O I
10.1002/adem.202302142
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Copper-based diamond composites are widely used for thermal management and wear-resistant materials. In this work, Cu/diamond, Cu/tungsten carbide (WC)/diamond, and Cu-0.92Cr/WC/diamond composites are fabricated by high-energy ball milling and rapid hot-pressing sintering. Physical characteristics, compressive strength, and tribological properties of the studied composites are investigated. The compressive strength of Cu/7wt%WC/diamond composites is 102% higher than the Cu/diamond composites, reaching 415 MPa. Compression fractures extend from the interface due to compression cracks, consistent with the compression curves from molecular dynamics (MD) simulations. The crack propagates from the interface during the compression experiment, which is consistent with the result of MD simulation. The Cu/7wt%WC/diamond composites exhibit a wear rate of 0.6 x 10-6 mm3 (N m)-1 and a friction coefficient of 0.37 at 50 N. The addition of WC and diamond improves the compressive strength and wear resistance. These findings are helpful in the development of copper composites with high compression strength and wear resistance. In this work, Cu-based composites with diamond and tungsten carbide (WC) are fabricated by high-energy ball milling and rapid hot-pressing sintering. As a result, the compressive strength of Cu/7 wt%WC/diamond composites is 102% higher than the Cu/diamond composites, reaching 415 MPa. The Cu/7wt%WC/diamond composite exhibits a wear rate of 0.6 x 10-6 mm3 (N m)-1 and a friction coefficient of 0.37.image (c) 2024 WILEY-VCH GmbH
引用
收藏
页数:12
相关论文
共 50 条
  • [1] High Strength and High Wear-Resistant Ti Composites Fabricated by Powder Metallurgy Pressureless Sintering
    Liu, Yanjun
    Pan, Yu
    Sun, Jianzhuo
    Kuang, Fan
    Yu, Aihua
    Yang, Shaofeng
    Zhang, Jiazhen
    Lu, Xin
    ADVANCED MATERIALS TECHNOLOGIES, 2022, 7 (11)
  • [2] High-strength and wear-resistant Co-Cr-Mo/diamond composites fabricated by selective laser melting
    Tao, Yakun
    Gan, Jie
    Sun, Wucheng
    Zhou, Yan
    Duan, Longchen
    Wen, Shifeng
    Shi, Yusheng
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2023, 113
  • [3] WEAR STUDIES OF NICKEL-TUNGSTEN CARBIDE-GRAPHITE COMPOSITES FABRICATED BY POWDER METALLURGY
    HIRSCHHO.JS
    DAVER, EM
    JOURNAL OF METALS, 1968, 20 (01): : A145 - +
  • [4] The Development of High-Strength Wear-Resistant Composites Based on UHMWPE and Nanodiamonds
    Gogoleva, O. V.
    Sharin, P. P.
    Petrova, P. N.
    Kolesova, E. S.
    Sivtseva, A. V.
    INORGANIC MATERIALS-APPLIED RESEARCH, 2024, 15 (01) : 183 - 189
  • [5] Ultrahigh strength CuCr/diamond composites fabricated by powder metallurgy
    Zhang, Xiaoyan
    Lei, Qian
    Yin, Jie
    Zhou, Shijie
    Xiao, Zhu
    Tang, Yulin
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2024, 122
  • [6] HIGH-TEMPERATURE WEAR-RESISTANT POWDER MATERIALS FOR METALLURGY
    MANEGIN, YV
    SURIKOVA, MA
    STEEL IN TRANSLATION, 1995, 25 (01) : 65 - 69
  • [7] High strength and high conductivity Cu-Ta composites fabricated by powder metallurgy
    Jiang, Haoze
    Li, Yangzhi
    Jiang, Long
    Zhang, Xiukuang
    Liu, Xiaoxu
    Li, Liwei
    Li, Lei
    Tian, Yingcheng
    Zhang, Li
    Guo, Junguang
    Lei, Qian
    MATERIALS TODAY COMMUNICATIONS, 2024, 38
  • [8] High thermal conductivity Cu-3Cr/Diamond composites fabricated by powder metallurgy
    Zhang, Xiaoyan
    Lei, Qian
    MATERIALS LETTERS, 2024, 363
  • [9] DEVELOPMENT OF AN OPTIMAL COMPOSITION OF THREE-COMPONENT HIGH-STRENGTH WEAR-RESISTANT COMPOSITES BASED ON POLYIMIDE
    S. V. Panin
    J. Luo
    D. G. Buslovich
    L. A. Kornienko
    V. O. Aleksenko
    S. A. Bochkareva
    Journal of Applied Mechanics and Technical Physics, 2021, 62 : 1028 - 1036
  • [10] DEVELOPMENT OF AN OPTIMAL COMPOSITION OF THREE-COMPONENT HIGH-STRENGTH WEAR-RESISTANT COMPOSITES BASED ON POLYIMIDE
    Panin, S., V
    Luo, J.
    Buslovich, D. G.
    Kornienko, L. A.
    Aleksenko, V. O.
    Bochkareva, S. A.
    JOURNAL OF APPLIED MECHANICS AND TECHNICAL PHYSICS, 2021, 62 (06) : 1028 - 1036