Cr2AlC and metals reactivity: Sintering and oxidation

被引:0
|
作者
Zuber, A. [1 ]
Gauthier-Brunet, V. [1 ]
Dubois, S. [1 ]
机构
[1] Univ Poitiers, CNRS, Inst PPRIME, ENSMA, Blvd M&P Curie,TSA 41126, F-86073 Poitiers 9, France
来源
OPEN CERAMICS | 2024年 / 17卷
关键词
Cr2AlC; MAX phase; Metal reactivity; Oxidation; High-temperature; Kinetic; Blistering; HIGH-TEMPERATURE OXIDATION; MAX PHASE; MICROSTRUCTURE EVOLUTION; MECHANICAL-PROPERTIES; TI3ALC2; TI2ALC; COMPOSITES; RESISTANCE; STRENGTH; TI3SIC2;
D O I
10.1016/j.oceram.2024.100561
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Cr2AlC-20 wt% (Sn; Cu; Co; Fe; Ag) powder mixtures were hot isostatically pressed at 1000 degrees C for 4 h under 150 MPa to investigate the possible alloying behaviour of the metals with the MAX phase. The as-synthesized bulk materials were further oxidized at 1000 and 1200 degrees C for 10 h under dry air flux to study the effect of the alloying on the oxidation performance of the MAX phase. The metallic elements did not dissolve into the MAX phase grains: they mainly acted as oxidizing agents on the MAX phase grains, draining the aluminum from it to form intermetallic phases. The oxidation tests resulted in the formation of an alumina scale for most of the samples. The oxidation kinetic study shows no improvement of the oxidation behaviour of the Cr2AlC-metal composites as compared to pure bulk Cr2AlC. Sn spheres embedded in an alumina layer and empty alumina shells are respectively observed on the surface of the oxidized Cr2AlC-Sn and Cr2AlC-Ag composites.
引用
收藏
页数:8
相关论文
共 50 条
  • [1] Nonisothermal sintering of Cr2AlC powder
    Rajkumar, Yembadi
    Rahul, Bapurao
    Akash, Puppala Ananth
    Panigrahi, Bharat
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2017, 14 (01) : 63 - 67
  • [2] Reaction Synthesis and Pressureless Sintering of Cr2AlC Powder
    Panigrahi, Bharat Bhooshan
    Chu, Min-Cheol
    Kim, Yong-Il
    Cho, Seong-Jai
    Gracio, Jose J.
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2010, 93 (06) : 1530 - 1533
  • [3] Oxidation of Cr2AlC at 1300 °C in air
    Lee, D. B.
    Nguyen, Thuan Dinh
    Han, J. H.
    Park, S. W.
    CORROSION SCIENCE, 2007, 49 (10) : 3926 - 3934
  • [4] Sintering mechanisms of ultrafine Cr2AlC MAX phase powder
    Rajkumar, Y.
    Panigrahi, Bharat B.
    MATERIALS TODAY COMMUNICATIONS, 2016, 8 : 46 - 52
  • [5] Sintering behavior of Cr2AlC MAX phase synthesized by Spark plasma sintering
    Zakeri-Shahroudi, Fatemeh
    Ghasemi, Behrooz
    Abdolahpour, Hassan
    Razavi, Mansour
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2022, 19 (03) : 1309 - 1318
  • [6] High-temperature oxidation and hot corrosion of Cr2AlC
    Lin, Z. J.
    Li, M. S.
    Wang, J. Y.
    Zhou, Y. C.
    ACTA MATERIALIA, 2007, 55 (18) : 6182 - 6191
  • [7] Oxidation of Cr2AlC Between 900 and 1200°C in Air
    Lee, D. B.
    Park, S. W.
    OXIDATION OF METALS, 2007, 68 (5-6): : 211 - 222
  • [8] Oxidation of Cr2AlC Between 900 and 1200 °C in Air
    D. B. Lee
    S. W. Park
    Oxidation of Metals, 2007, 68 : 211 - 222
  • [9] A Critical Review of the Oxidation of Ti2AlC, Ti3AlC2 and Cr2AlC in Air
    Tallman, Darin J.
    Anasori, Babak
    Barsoum, Michel W.
    MATERIALS RESEARCH LETTERS, 2013, 1 (03): : 115 - 125
  • [10] SPS and HP-HT Sintering and Characterization of Cr2AlC Matrix Composites
    Jaworska, L.
    Bucko, M.
    Stobierski, L.
    Krolicka, B.
    Kalinka, A.
    JOURNAL OF THE AUSTRALIAN CERAMIC SOCIETY, 2013, 49 (01) : 7 - 8