摘要
The compliance of the tip-sample contact region in a scanning tunneling/atomic force microscope (STM/AFM) is found to increase from — 1 N/m to more than 200 N/m with decreasing tip-to-surface distance in a distance interval of — 200 nm. When a tungsten tip and a metal sample are used, this interval includes the distance at which a tunneling current is measurable. An STM/AFM was operated at this tip-to-surface distance in the constant-compliance mode. Since a tunneling contact to the tip is established at conducting sections of the sample, the electrical potential can be measured there. An array of interconnected niobium squares and an array of metal strips alternately connected to two electrodes of different voltage were examined using this method. Both structures were fabricated by electron beam lithography from Nb films on oxidized Si substrates. The topography and the value of the electrical potential were recorded. A potential resolution of the order of 1 mV was achieved. © 1990, American Vacuum Society. All rights reserved.
引用
收藏
页码:394 / 399
页数:6
相关论文
共 50 条
  • [1] Thin-film friction and adhesion studies using atomic force microscopy
    Bhushan, B
    Dandavate, C
    [J]. JOURNAL OF APPLIED PHYSICS, 2000, 87 (03) : 1201 - 1210
  • [2] ATOMIC-FORCE MICROSCOPY FOR THIN-FILM ANALYSIS
    PHILLIPS, RW
    [J]. SURFACE & COATINGS TECHNOLOGY, 1994, 68 : 770 - 775
  • [3] Potential mapping of pentacene thin-film transistors using purely electric atomic-force-microscope potentiometry
    Nakamura, M
    Goto, N
    Ohashi, N
    Sakai, M
    Kudo, K
    [J]. APPLIED PHYSICS LETTERS, 2005, 86 (12) : 1 - 3
  • [4] Thin-film hydrodynamics in fluid interface-atomic force microscopy
    Aston, DE
    Berg, JC
    [J]. INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2002, 41 (03) : 389 - 396
  • [5] ATOMIC AND MAGNETIC FORCE MICROSCOPY IMAGING OF THIN-FILM RECORDING-HEADS
    CHIM, WK
    [J]. SCANNING, 1995, 17 (05) : 306 - 311
  • [6] Atomic force acoustic microscopy methods to determine thin-film elastic properties
    Hurley, DC
    Shen, K
    Jennett, NM
    Turner, JA
    [J]. JOURNAL OF APPLIED PHYSICS, 2003, 94 (04) : 2347 - 2354
  • [7] MAGNETIC FORCE MICROSCOPY OF A COCR THIN-FILM
    GRUTTER, P
    WADAS, A
    MEYER, E
    HIDBER, HR
    GUNTHERODT, HJ
    [J]. JOURNAL OF APPLIED PHYSICS, 1989, 66 (12) : 6001 - 6006
  • [8] Chemical imaging of patterned inorganic thin-film structures by lateral force microscopy
    Utriainen, M
    Leijala, A
    Niinistö, L
    Matero, R
    [J]. ANALYTICAL CHEMISTRY, 1999, 71 (13) : 2452 - 2458
  • [9] Calculation of the thicknesses and elastic properties of thin-film coatings using atomic-force acoustic microscopy data
    Batog, G. S.
    Baturin, A. S.
    Bormashov, V. S.
    Sheshin, E. P.
    [J]. TECHNICAL PHYSICS, 2006, 51 (08) : 1084 - 1089
  • [10] Calculation of the thicknesses and elastic properties of thin-film coatings using atomic-force acoustic microscopy data
    G. S. Batog
    A. S. Baturin
    V. S. Bormashov
    E. P. Sheshin
    [J]. Technical Physics, 2006, 51 : 1084 - 1089