ROLLING TEXTURES OF PURE NICKEL, NICKEL-IRON AND NICKEL-COBALT ALLOYS

被引:99
|
作者
RAY, RK
机构
[1] Department of Materials and Metallurgical Engineering, Indian Institute of Technology, Kanpur
来源
ACTA METALLURGICA ET MATERIALIA | 1995年 / 43卷 / 10期
关键词
D O I
10.1016/0956-7151(95)90169-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The rolling texture of heavily rolled pure Ni has been found to be similar to the rolling texture of deformed pure Cu. The textures of Ni-Fe alloys with up to 40% Fe, are similar amongst themselves and also to that of pure Ni. The Ni-Co alloys with up to 30% Co show pure metal-type rolling texture, while the Ni-60% Co alloy shows alloy-type texture. The rolling texture of the Ni-40% Co alloy lies in between these two extremes. The similarity of the deformation textures of pure Ni and Ni-Fe alloys can be explained due to only a marginal variation of the stacking-fault energy of Ni as a function of Fe-content. The texture transition in the Ni-Co alloys has been attributed to the additional effect of the incidence of twinning caused by the sharp decrease of stacking fault energy of Ni by Co-addition.
引用
收藏
页码:3861 / 3872
页数:12
相关论文
共 50 条