共 5 条
- [1] ADSORPTION, FACETING, AND INITIATION OF OXIDATION ON PURE IRON UNDER WATER VAPO R HYDROGEN MIXTURES AT 900 TO 1200 DEGREES C [J]. ARCHIV FUR DAS EISENHUTTENWESEN, 1974, 45 (06): : 395 - 403
- [2] THE ROLE OF HYDROGEN IN CORROSION FATIGUE OF HIGH-PURITY AL-ZN-MG EXPOSED TO WATER-VAPOR [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1988, 19 (07): : 1775 - 1783
- [3] EQUILIBRIUM HYDROGEN-WATER VAPOR RATIOS OVER IRON-CHROMIUM ALLOY CHROMIUM OXIDE AND IRON CHROMITE FROM 900 DEGREES TO 1200 DEGREES C [J]. TRANSACTIONS OF THE METALLURGICAL SOCIETY OF AIME, 1966, 236 (04): : 559 - +