- [1] EXPERIENCES WITH THE PRODUCTION OF SEAMLESS TUBES FROM HIGH-ALLOY STEELS [J]. NEUE HUTTE, 1986, 31 (08): : 291 - 297
- [2] INTENSIFICATION OF PROCESS OF APPLYING COPPER COATING TO HIGH-ALLOY STEEL TUBES [J]. STEEL IN THE USSR, 1981, 11 (02): : 99 - 99
- [3] Application of EAF wall injectors for high-alloy steel production [J]. Iron and Steel Technology, 2018, 15 (01): : 42 - 49
- [4] ON THE FORMABILITY OF HIGH-ALLOY STEEL TUBES DURING COLD PILGER ROLLING [J]. NEUE HUTTE, 1983, 28 (09): : 325 - 328
- [5] PRODUCTION OF HIGH-ALLOY STEEL TUBES WITH SMALL DIAMETER ACCORDING TO THE GTA METHOD [J]. NEUE HUTTE, 1983, 28 (09): : 337 - 341
- [7] Activation of high-alloy steel cathodes [J]. RUSSIAN JOURNAL OF APPLIED CHEMISTRY, 1998, 71 (07) : 1181 - 1184
- [9] Laser hardening of high-alloy steel [J]. 20TH CHEMNITZ SEMINAR ON MATERIALS ENGINEERING, 2018, 373
- [10] PROPERTIES AND STRUCTURE OF HIGH-ALLOY STEEL [J]. RUSSIAN ENGINEERING JOURNAL-USSR, 1965, 45 (12): : 62 - &